SC626 Anti-Aging Two-Component Epoxy — Wide-Temp Cycling, Chemical-Resistant, High Peel Strength Insulating Adhesive
QUALITY CONTROL100% Lab Tested
DISPENSING SPECNordson Syringe
OUTER PACKAGINGVacuum-Sealed
PACKAGING SPEC50ml/syringe
THE INVISIBLE INTERFACE

SC626 Anti-Aging Two-Component Epoxy — Wide-Temp Cycling, Chemical-Resistant, High Peel Strength Insulating Adhesive

Anti-aging two-component epoxy series. All −55 °C Mil-Std compliant, 280 °C, solvent resistant, high peel strength. Multiple grades for complex cycling conditions. Damp-heat storage 720 h (70 °C / 95% RH): 92% shear retention; damp-heat storage 1000 h (85 °C / 85% RH): 70% shear retention.

Typical Application

Military sensors, military-standard parts and automotive-grade parts — bonding, sealing, filling and insulation.

Technical Specifications
Shear Strength
32 MPa
Temperature Range
−55 °C–280 °C
Cure Condition
RT or heat cure
Viscosity @ 25 °C
8000–80000 mPa·s
* Multiple specifications are available for this series
SCITEO Rigorous Standards: Qualified under GJB 150 environmental reliability testing by Zhenhua, CETC, and CAC, delivering mission-critical reliability.

Engineered as high-reliability domestic qualified alternatives for semiconductor and defense manufacturing clusters across Shanghai Zhangjiang, Xi'an, Chengdu, and Wuxi.

SCITEO R&D ARCHIVE

Specifications Don't Match Your Operating Conditions?

Only the baseline series is shown here. SCITEO's undisclosed archive holds formulations engineered for extreme environments. Contact us — our application engineers will match you precisely.

Contact Below
APPLICATION FIELDS

High Reliability Scenarios

Core positioning and partial application demonstration of this product under complex operating conditions.

SCITEO anti-aging epoxy AB adhesive for semiconductor power module bonding and sealing

Power Module Bonding

SCITEO anti-aging epoxy AB adhesive for heat dissipation component copper-aluminum bonding, sealing and filling

Heat-Dissipation Component Bonding

SCITEO anti-aging epoxy AB adhesive for military-standard component bonding, sealing, filling and insulation

Military Component Bonding

FAQ & ENGINEERING ANSWERS

Application Engineer FAQ

A structured brief from SCITEO covering physical properties, application standards, and related specifications.

Q

What substrates does SC626 bond? Strength?

A

Bonds plastics, metals, glass, ceramics, and platings: ~30 MPa room-temperature shear, ~6,000 MPa dynamic modulus, and >6 N/mm T-peel, delivering vibration, creep, and crack resistance.

Q

Anti-aging performance?

A

SC626 holds 32 MPa after 720 h in 5% neutral salt spray and oil immersion, and 22 MPa after 720 h of heat aging at 155 °C; damp-heat aging leaves ample strength margin.

Engineering Support

Request Technical Documentation or Consult an Application Engineer

Receive product documentation and customized formulations. Please provide accurate information for verification.